We use cookies to ensure that we give you the best experience on our website. If you click 'Accept all cookies' we'll assume that you are happy to receive all cookies and you won't see this message again. If you click 'Reject all non-essential cookies' only necessary cookies providing core functionality such as security, network management, and accessibility will be enabled. Click 'Find out more' for information on how to change your cookie settings.

A study was conducted to determine weight loss and moisture regain properties of silk cocoon shells, shell layers and degummed fibers of the four African wild silkmoths Anaphe panda, Argema mimosae, Epiphora bauhiniae and Gonometa postica and compare with the industry standard mulberry silkmoth, Bombyx mori. No. significant difference was observed between the moisture regain of the wild silk fibers after degumming. However, there were significant differences in weight loss and moisture regain between cocoon shells as well as shell layers. E. bauhiniae had the lowest weight loss and moisture regain of 23.19 and 5.64%, respectively while G. postica had the highest weight loss and moisture regain, 56.84 and 9.05%, respectively. The SEM micrographs also showed the presence of remnant sericin gum on the fibers surface. In both A. panda and E. bauhiniae, the outer shell layers had the lowest moisture regain and highest weight loss while the inner layer of E. bauhiniae and middle layer of A. panda lost the least weight. The physical structure and chemical composition of the cocoon shells and fibers contribute towards the variation in the moisture regain and weight loss and these features may have commercial implications due to their direct effect on the resulting fabric. © 2011 Academic Journals Inc.

Original publication

DOI

10.3923/je.2011.450.458

Type

Journal article

Journal

Journal of Entomology

Publication Date

01/06/2011

Volume

8

Pages

450 - 458